FIELD: electrical engineering. SUBSTANCE: one contact of contact pair is manufactured from metal ceramics, parts by mass: silver 97; graphite being the balance. Second contact is fabricated from heat-resistant copper alloy, parts by mass: chrome 0.4-0.7; copper being the balance with galvanic silver coat. EFFECT: use of contact pair provides for stable low contact resistance.
| Title | Year | Author | Number |
|---|---|---|---|
| CONTACT PAIR | 0 |
|
SU1735927A1 |
| CHARGE PREPARING METHOD | 1988 |
|
SU1577173A1 |
| METAL-CERAMIC BIMETAL ELECTRIC CONTACT | 1985 |
|
SU1313244A1 |
| METHOD OF PRODUCING COMPOSITE MATERIAL FOR COPPER-BASED ELECTRIC CONTACTS | 2009 |
|
RU2398656C1 |
| CERMET BIMETALLIC ELECTRIC CONTACT | 0 |
|
SU1107184A1 |
| ELECTRIC CONTACT | 2017 |
|
RU2644414C1 |
| BIMETALLIC CERMET ELECTRIC CONTACT | 1988 |
|
SU1524734A1 |
| HETEROGENEOUS CONTACT PAIR | 1984 |
|
SU1210596A1 |
| METHOD OF MANUFACTURING ELECTRIC CONTACTS | 0 |
|
SU1746418A1 |
| ARC-RESISTANT ELECTRIC CONTACT | 1992 |
|
RU2007772C1 |
Authors
Dates
1995-06-09—Published
1992-12-18—Filed