FIELD: powder metallurgy. SUBSTANCE: material has working layer made of a compound based on silver containing cadmium oxide in the amount of 12 to 17 percent, process layer made of a compound of sliver-copper at the following relation of constituents, mass percent: silver - 26 to 34, copper - 66 to 74. The service life of contacts made of the offered material is 1 700 000 to 1 630 000 ON/OFF cycles. Consumption of silver decreases by 6 to 11.5%. EFFECT: reduced cost of material, with service life remaining unchanged. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METAL-CERAMIC BIMETAL MATERIAL FOR ELECTRIC CONTACTS | 1984 |
|
SU1415970A1 |
MIXTURE FOR PROCESS PRECOAT OF CERMET SILVER-CONTAINING CONTACT | 1989 |
|
SU1605861A1 |
BIMETAL METAL-CERAMIC MATERIAL FOR ELECTRIC CONTACTS | 1985 |
|
SU1272909A1 |
METAL-OXIDE MATERIAL FOR BURSTING ELECTRIC CONTACTS | 2008 |
|
RU2367695C1 |
METAL-CERAMIC BIMETALLIC ELECTRIC CONTACT | 0 |
|
SU907602A1 |
LAMINATED ELECTRIC CONTACT | 2002 |
|
RU2221299C1 |
METHOD OF APPLICATION OF ELECTROEROUSION-RESISTANT COATINGS BASED ON OXIDE CADMIUM AND SILVER ONTO COPPER ELECTRICAL CONTACTS | 2017 |
|
RU2663022C1 |
LAMINATED ELECTRIC CONTACT | 2002 |
|
RU2228557C1 |
BIMETALLIC CERMET ELECTRIC CONTACT | 1988 |
|
SU1524734A1 |
METHOD OF PRODUCING POWDER CERAMET Cu-Cd/CdO FOR ELECTRIC CONTACTS | 2009 |
|
RU2401314C1 |
Authors
Dates
1995-04-20—Published
1987-05-04—Filed