FIELD: ferrous metallurgy. SUBSTANCE: tungsten-containing oxide wastes are charged after melting through of the first portion in mixture with calcium hydroxide or carbonate with mixture component ratio of 1:(0.01-0.1) in the amount of 0.02-0.1 from the weight of the first portion. EFFECT: higher recovery of tungsten and reduced material costs for smelting due to reduced amount of return metal wastes. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR ALUMINIUM-SILICON-THERMAL PRODUCTION OF FERRO-TUNGSTEN | 2008 |
|
RU2411299C2 |
CHARGE AND METHOD FOR ALUMINOTHERMIC PRODUCTION OF FERROMOLYBDENUM USING IT | 2012 |
|
RU2506338C1 |
CHARGE AND METHOD FOR ELECTRIC-FURNACE ALUMINOTHERMIC PRODUCTION OF FERROBORON USING IT | 2013 |
|
RU2521930C1 |
CHARGE AND ELECTRIC FURNACE METHOD OF PRODUCING FERROBORON WITH ITS USE | 2019 |
|
RU2719828C1 |
METHOD FOR PREPARING METALLOTHERMIC MELT FOR PREPARATION OF MASTER ALLOY CONTAINING MOLYBDENIUM AND TUNGSTEN | 0 |
|
SU1129262A1 |
METHOD OF ALUMINOTHERMIC SMELTING OF FERROTUNGSTEN | 0 |
|
SU1013504A1 |
METHOD OF PRODUCING FERROTUNGSTEN FROM TUNGSTEN CONCETRATES | 0 |
|
SU1217910A1 |
METHOD OF PRODUCING FERROMOLYBDENUM BY METAL-THERMAL PROCESS | 0 |
|
SU1235964A1 |
METHOD FOR PRODUCING FERROMOLYBDENUM | 1994 |
|
RU2110596C1 |
CHARGE AND ELECTRIC FURNACE ALUMINOTHERMIC METHOD FOR PRODUCING LOW-CARBON FERROCHROME WITH ITS USE | 2021 |
|
RU2761839C1 |
Authors
Dates
1995-08-20—Published
1990-06-27—Filed