FIELD: alloy working. SUBSTANCE: articles were subjected for heating up to 920-950 C at the rate 100 C/s (not less), kept at this temperature for 10-15 s, cooled up to the room temperature at the rate 450-1200 C/s at the range of temperature 920-500 C followed by annealing at 580-540 C for 24-100 h, respectively. This working improves creeping and corrosion resistance due to making quasi-isotropic fine-grained structure. EFFECT: improved method of working. 4 tbl, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
NUCLEAR FUEL ASSEMBLY TUBE AND ITS MANUFACTURING PROCESS | 1996 |
|
RU2172527C2 |
METHOD OF PRODUCING PRODUCTS FROM THE ZIRCONIUM ALLOYS | 1993 |
|
RU2032760C1 |
METHOD OF THERMOMECHANICAL MACHINING OF STRUCTURAL TUBING SHAPE MADE OUT O F BINARY ZIRCONIUM-NIOBIC ALLOYS | 2003 |
|
RU2230134C1 |
METHOD OF FABRICATION OF SEMI-FINISHED PRODUCT OUT OF ZIRCONIUM ALLOY AND IMPLEMENTATION OF SEMI-FINISHED PRODUCT | 2004 |
|
RU2337177C2 |
ZIRCONIUM-BASED ALLOY RESISTANT TO FLOWABILITY AND CORROSION | 1997 |
|
RU2199600C2 |
ZIRCONIUM BASE ALLOY TUBE FOR NUCLEAR REACTOR FUEL ASSEMBLY | 1996 |
|
RU2126559C1 |
METHOD FOR MANUFACTURING TUBULAR PRODUCTS FROM ZIRCONIUM-BASED ALLOY | 2019 |
|
RU2798022C1 |
METHOD FOR PRODUCING THIN COMPONENTS FROM ZIRCONIUM BASE ALLOY AND PLATES PRODUCED BY THIS METHOD | 2000 |
|
RU2239892C2 |
ZIRCONIUM-BASE ALLOY | 1999 |
|
RU2141539C1 |
METHOD OF PLATE WORKPIECE RECEIVING FROM ZIRCONIUM ALLOY, RECEIVED BY THIS METHOD PLATE WORKPIECE AND THE ELEMENT OF FUEL ASSEMBLY OF NUCLEAR REACTOR OF NUCLEAR POWER PLANT, MADE OF PLATE WORKPIECE | 2004 |
|
RU2350684C2 |
Authors
Dates
1995-08-27—Published
1989-12-25—Filed