FIELD: nonferrous metallurgy. SUBSTANCE: solution of perfluorinated surface-active substance is added to sulfate or sulfate-chloride electrolyte for electrodeposition of nickel. Before feeding to electrolyte surface-active substance is chlorinated by bubbling of chlorine through its at concentration 0,15-0,3 hm3 per 1 kg surface-active substance in solution. Then prepared electrolyte is fed for nickel electrodeposition. EFFECT: improved method of nickel production. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF NICKEL | 1994 |
|
RU2066713C1 |
NICKEL ELECTROLYTIC PRODUCTION METHOD | 2003 |
|
RU2247796C1 |
METHOD OF NICKEL PRODUCTION | 0 |
|
SU1788089A1 |
ELECTROLYTE FOR CHROMIUM-PLATING OF STEELS, COPPER AND TITANIUM ALLOYS | 2001 |
|
RU2187587C1 |
PROCESS OF PREPARATION OF ELECTROLYTE FOR DEPOSITION OF METAL NICKEL ( VERSIONS ) | 1998 |
|
RU2132889C1 |
CATHODE COPPER TO PRODUCE COPPER CASTINGS AND ROLLED STOCK AND PROCESS OF ITS WINNING ( VARIANTS ) | 2000 |
|
RU2180019C2 |
METHOD OF ELECTROCHEMICAL DEPOSITION OF PERMALLOY FILMS NiFe FOR INTEGRATED CIRCUITS | 2018 |
|
RU2710749C1 |
ELECTROLYTE FOR CHROMIUM PLATING OF TITANIUM ALLOYS | 0 |
|
SU1114712A1 |
METHOD FOR PREPARING ELECTROLYTE FOR ELECTROLYTIC REFINING OF COPPER | 2004 |
|
RU2280106C2 |
METHOD OF ELECTROLYTICAL REFINING OF NICKEL | 0 |
|
SU1514831A1 |
Authors
Dates
1995-04-10—Published
1991-01-17—Filed