FIELD: preparing aqueous suspension of microsilica. SUBSTANCE: powder microsilica (being waste of ferroalloy production and having specific surface 20 m2/g) is mixed with 0.03-0.3% aqueous solution of nitriletrimethylenephosphoric acid to produce 50-60% suspension. Viscosity thus prepared suspension is 0.8-1.0 P. EFFECT: increases stability and fluidity of suspension, decreases its aggressive action against metal. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING MICROSILICA AQUEOUS SUSPENSION | 1994 |
|
RU2085542C1 |
GLASS-FIBER-CONCRETE MIXTURE | 1990 |
|
SU1811681A1 |
METHOD OF PREPARING OF COMPLEX ADDITION FOR CONCRETE MIXTURE | 1992 |
|
RU2033403C1 |
LUBRICANT FOR METAL MOULDS | 1991 |
|
RU2035300C1 |
CONCRETE MIX | 1992 |
|
RU2057098C1 |
COMPLEX ADDITION FOR CONCRETE MIXTURE | 1992 |
|
RU2041863C1 |
METHOD OF CONCRETE MIXTURE PREPARATION | 2013 |
|
RU2530967C1 |
METHOD OF PREPARING CONCRETE MIX | 1996 |
|
RU2095327C1 |
MIX FOR MANUFACTURING HEAT-INSULATING PRODUCTS | 1999 |
|
RU2169132C1 |
METHOD OF TREATING CONCRETE SURFACES | 1995 |
|
RU2078691C1 |
Authors
Dates
1994-05-30—Published
1991-02-01—Filed