FIELD: industry of building materials. SUBSTANCE: glass-fiber-concrete mixture has, wt. -% : portland cement 20-24; fiber glass 1-3.5; small filler 40; ultra-dispersed waste in production of crystalline silicon and ferroalloys 16-20; superplasticizer 16-20, and water - the rest. Mixture is prepared by stirring of components. Enhanced corrosion resistance of concrete obtained is accompanied by decrease of strength but not more than 2% in samples for long storage (up to 500 days) as compared with 28 days old concrete. EFFECT: enhanced corrosion resistance of concrete. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
CONCRETE MIX | 1992 |
|
RU2057098C1 |
CONCRETE MIXTURE | 1993 |
|
RU2064907C1 |
COMPLEX ADDITION FOR CONCRETE MIXTURE | 1992 |
|
RU2041863C1 |
CONCRETE MIXTURE | 0 |
|
SU1696406A1 |
METHOD OF PRODUCING CONCRETE MIX | 0 |
|
SU1675285A1 |
METHOD OF PREPARING OF COMPLEX ADDITION FOR CONCRETE MIXTURE | 1992 |
|
RU2033403C1 |
MIX FOR MANUFACTURING HEAT-INSULATING PRODUCTS | 1999 |
|
RU2169132C1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2022 |
|
RU2806385C1 |
SEAMLESS POURED-IN-PLACE CONCRETE FLOOR | 1998 |
|
RU2137730C1 |
METHOD OF CONCRETE MIXTURE PREPARING | 1991 |
|
RU2016885C1 |
Authors
Dates
1994-04-30—Published
1990-04-18—Filed