FIELD: concrete mixtures. SUBSTANCE: complex addition for concrete mixture has, superplasticizer C-3 on the basis of sodium salt of product condensation of β-naphthalenesulfoacid with formaldehyde 85.21-89.74; alkylsulfate 7.26-10.65; neutral lipids waste of production of protein-vitamin concentrates 3.0-4.14. Concrete strength limit at 28 days with addition is: at compression up to 70.5 MPa, at bending up to 9.8 MPa. Water-proofing quality up to 12. EFFECT: enhanced quality of addition. 2 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| CONCRETE MIX | 1992 | 
 | RU2057098C1 | 
| CONCRETE MIXTURE | 1993 | 
 | RU2064907C1 | 
| GLASS-FIBER-CONCRETE MIXTURE | 1990 | 
 | SU1811681A1 | 
| METHOD OF PREPARING OF COMPLEX ADDITION FOR CONCRETE MIXTURE | 1992 | 
 | RU2033403C1 | 
| CEMENT COMPOSITION | 1992 | 
 | RU2090531C1 | 
| MIX FOR MANUFACTURING HEAT-INSULATING PRODUCTS | 1999 | 
 | RU2169132C1 | 
| CONCRETE MIXTURE | 0 | 
 | SU1696406A1 | 
| EXPANDING ADDITION TO PORTLAND CEMENT | 1992 | 
 | RU2049079C1 | 
| DRY MORTAR MIXTURE | 2002 | 
 | RU2214376C1 | 
| METHOD OF CONCRETE MIXTURE PREPARING | 1991 | 
 | RU2016885C1 | 
Authors
Dates
1995-08-20—Published
1992-12-29—Filed