FIELD: ceramics. SUBSTANCE: solution has hydrogen peroxide, magnesium oxide, silicon oxide as an aerosil, magnesium or aluminium or together magnesium and aluminium at the following ratio of components, wt.-% ortho-phosphoric acid 10-27; chrome anhydride 3-10; 30% solution hydrogen peroxide 2-8; aerosil 2-8; magnesium oxide 1-3; magnesium or aluminium or sum of magnesium and aluminium 0.8-2.0, and water 81.2-42 at the ratios: Al+Mg/H3PO4- 0.07-0.08; SiO2/H3PO4= 0.2-0.3; 30% H2O2/CrO3= 0.4-0.8. Working life os solution is increased from 3 days ad infinitum. Film thickness is increased from 0.5-3.0 mcm at 2-10-fold treatment to 10 mcm at single-stage that decreases labor consumption by 2-4-fold. EFFECT: enhanced quality of material, decreased cost. 3 cl, 4 tbl
Title | Year | Author | Number |
---|---|---|---|
PIECES PROTECTION COVER APPLICATION METHOD | 1993 |
|
RU2036978C1 |
SUSPENSION FOR ALUMINO-SILICONIZING OF METAL ARTICLES | 1993 |
|
RU2032764C1 |
COMPOSITION FOR OBTAINING PROTECTIVE COATING ON STEEL PARTS | 2012 |
|
RU2480534C1 |
SUSPENSION FOR GRAPHITE COATING PRODUCTION | 0 |
|
SU1806117A3 |
SUSPENSION FOR ALUMINIUM CHROMOSILICONISING OF PARTS MADE OF HEAT-RESISTANT NICKEL ALLOYS | 2006 |
|
RU2326183C1 |
METHOD OF APPLYING PROTECTIVE COATING ON STEEL COMPONENTS | 2012 |
|
RU2510716C2 |
METHOD OF APPLYING PROTECTIVE COATINGS | 0 |
|
SU1560621A1 |
METHOD TO PRODUCE ELECTRIC INSULATION COATING OF TRANSFORMER STEEL | 2011 |
|
RU2463384C1 |
COMPOSITION OF COMPOSITE FOR APPLYING OF METAL CONVERSION COATING ON METALLIC SURFACE | 1994 |
|
RU2094529C1 |
METHOD OF RESTORATION OF HEAT-RESISTANT THERMODIFFUSION ALUMINIDE COATINGS OF GAS TURBINE BLADES OF COMPLEX CONFIGURATION | 2007 |
|
RU2365478C2 |
Authors
Dates
1995-08-27—Published
1991-11-21—Filed