FIELD: chemical industry. SUBSTANCE: method provides for usage as binder for suspension of composition, that is used for production of glass ceramic film, made of following components, mass %: H3PO4 10 - 27; CrO3 10; 30 % solution of H2O2 2 - 8; SiO2 2 - 8; MgO 1 - 3; Al 0.2 - 1; H2O 81.8 - 43 with SiO2/H3PO4 0.2 - 0.3; 30 % H2O2/CrO3 0.4 - 0.8; Al / H3PO4 0.009 - 0.045. To produce suspension the solution is added with aluminum or its alloys powder in ratio solution / powder as 35 - 65 / 65 - 35 and to stop reaction of solution with powder suspension is heated for short time to 30 - 70 C. EFFECT: simplified process of suspension preparation, increased ecological purification of suspension usage, decreased temperature of heat treatment. 5 tbl
Title | Year | Author | Number |
---|---|---|---|
SUSPENSION FOR ALUMINO-SILICONIZING OF METAL ARTICLES | 1993 |
|
RU2032764C1 |
GLASS CERAMIC FILM ON METALLIC MEMBERS | 1991 |
|
SU1835129A3 |
SUSPENSION FOR GRAPHITE COATING PRODUCTION | 0 |
|
SU1806117A3 |
SUSPENSION FOR ALUMINIUM CHROMOSILICONISING OF PARTS MADE OF HEAT-RESISTANT NICKEL ALLOYS | 2006 |
|
RU2326183C1 |
METHOD OF APPLYING PROTECTIVE COATING ON STEEL COMPONENTS | 2012 |
|
RU2510716C2 |
COMPOSITION FOR OBTAINING PROTECTIVE COATING ON STEEL PARTS | 2012 |
|
RU2480534C1 |
METHOD OF APPLYING PROTECTIVE COATINGS | 0 |
|
SU1560621A1 |
METHOD OF PRODUCING OF FILTRATION MATERIAL | 2013 |
|
RU2579713C2 |
PROCEDURE FOR APPLICATION OF CORROSION-RESISTANT COATING OF ALUMINIUM OXIDE ON METAL ITEM | 2010 |
|
RU2430993C1 |
FABRICATION OF HEAT-BARRIER PROTECTION AND SANDWICHED COATING THAT CAN GENERATE SAID HEAT BARRIER | 2011 |
|
RU2561550C2 |
Authors
Dates
1995-06-09—Published
1993-05-18—Filed