FIELD: ferrous metallurgy, manufacture of structural alloys. SUBSTANCE: alloy includes the following components, % by weight: carbon 0.01-0.1; aluminum 4-12; manganese 0.3-3.0; titanium 0.01-1.0 and iron as the balance, with [Al-Σ(Mn+Ti)] 1% = 3.5-8.5. EFFECT: high damping index and mechanical characteristics. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
HIGH-DAMPING ALLOY BASED ON IRON WITH CONTROLLED LEVEL OF DAMPING AND MECHANICAL PROPERTIES AND PRODUCT MADE ON HIGH-DAMPING ALLOY | 1999 |
|
RU2158318C1 |
METHOD OF DEFORMATION-HEAT TREATMENT OF ALLOYS | 0 |
|
SU1772177A1 |
HIGH DAMPING STEEL WITH A SPECIFIED LEVEL OF DAMPING PROPERTIES AND AN ARTICLE MADE FROM IT | 2018 |
|
RU2685452C1 |
DAMPING STEEL AND ITEM MADE FROM IT | 2016 |
|
RU2623947C1 |
HIGH-DAMPING STEEL WITH THE REQUIRED LEVEL OF DAMPING PROPERTIES AND ARTICLE MADE THEREFROM | 2019 |
|
RU2721262C1 |
STAINLESS STEEL WITH HIGH DAMPING PROPERTIES | 1992 |
|
RU2025533C1 |
METHOD OF MANUFACTURING ARTICLE FROM FERRITE-CLASS DAMPING ALLOY AND ARTICLE MANUFACTURED BY THIS METHOD | 2001 |
|
RU2219252C2 |
RAIL STEEL | 2001 |
|
RU2194791C1 |
MANGANESE BASED ALLOY | 0 |
|
SU1836477A3 |
NITROGEN-CONTAINING IRON BASED-ALLOYS HAVING PROPERTIES OF DAMPING AND EFFECT OF MEMORY OF SHAPE | 1996 |
|
RU2169786C2 |
Authors
Dates
1994-01-15—Published
1992-04-01—Filed