FIELD: ferrous metallurgy. SUBSTANCE: wet scrubbing sludges are premixed with limestone to obtain the mixture humidity of 8-10% . The bentonite is added to the mixture to obtain the proportion of iron, calcium, silicon, and solid carbon oxides of 1 : (1.4-2) : (0.3-0.7) : (0.1-0.3), respectively. The product is crushed and mixed with iron ore concentrate in the proportion of 1 : (0.9-19). EFFECT: improved quality of the product. 6 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| BURDEN FOR PELLETS PRODUCTION | 1992 |
|
RU2009223C1 |
| METHOD FOR PREPARATION OF A SINTER BURDEN | 1992 |
|
RU2009220C1 |
| BURDEN FOR SINTER PRODUCTION | 1992 |
|
RU2009221C1 |
| IRON-ORE PELLET OBTAINING METHOD | 2013 |
|
RU2542186C1 |
| METHOD FOR PRODUCING PELLETS FROM ORE MATERIALS | 2022 |
|
RU2782595C1 |
| CHARGE FOR THE PRODUCTION OF MAGNESIAN IRON FLUX | 2022 |
|
RU2796485C1 |
| BATCH FOR PELLET PRODUCTION USED IN METALLURGY | 2003 |
|
RU2245930C1 |
| METHOD FOR PREPARING OF SINTER BURDEN FOR SINTERING TREATMENT | 2005 |
|
RU2313588C2 |
| METHOD OF PRODUCING IRON ORE PELLETS | 2023 |
|
RU2820429C1 |
| METHOD FOR PRODUCING FLUXED LUMPY MATERIAL | 0 |
|
SU1296615A1 |
Authors
Dates
1994-03-15—Published
1992-04-15—Filed