FIELD: metallurgy.
SUBSTANCE: components of the charge containing a binding agent in the form of a mixture of bentonite and red mud, and an iron-ore concentrate are dosed and mixed. Pelletisation of the prepared charge and firing of raw pellets is performed. First, red mud is dealkalised with a lime mortar till alkali content is less than 1% and charge in the quantity of 1.0-2.5 wt % is added. Pelletisation is performed at charge humidity of 8.0-9.3 wt %. Ratio of red mud and bentonite in the binding agent is maintained within 2.3-11.4.
EFFECT: invention allows reducing the quantity of the binding agent used in the charge at maintenance of high strength properties of the obtained product and prevention of environmental pollution.
4 cl, 3 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PELLETIZING MIXTURE | 1991 |
|
RU2023033C1 |
CHARGE FOR PELLET PRODUCTION | 1992 |
|
RU2031155C1 |
BINDING ADDITIVE FOR IRON ORE MATERIAL | 0 |
|
SU1008259A1 |
METHOD FOR PRODUCING PELLETS FROM ORE MATERIALS | 2022 |
|
RU2782595C1 |
METHOD FOR PRODUCTION OF PELLETS FOR BLAST FURNACE PLANT | 1992 |
|
RU2009222C1 |
FEEDSTOCK FOR PRODUCING PELLETS | 0 |
|
SU1742343A1 |
METHOD OF MAKING PELLETS FOR METALLURGY | 2011 |
|
RU2487952C1 |
METHOD FOR PELLETIZING IRON ORE CONCENTRATES | 1992 |
|
RU2034055C1 |
METHOD OF MAKING PELLETS FOR REDUCTION CASTING | 2010 |
|
RU2459879C2 |
BINDER FOR PELLETIZING IRON ORE MATERIALS | 0 |
|
SU1654351A1 |
Authors
Dates
2015-02-20—Published
2013-08-06—Filed