FIELD: nuclear plant and environment decontaminating technology. SUBSTANCE: glass powder and clay are added to liquid waste and mixture is boiling down until residual moisture factor goes to 20-30% , then mixture is granulating and heating. After this processing granulated product is admixed to chrome-iron ore and it is calcining at temperature 600-650 C to initiate self-propagating high-temperature processing of ceramic synthesis. Method permits to produce desirable product which has better waterproofness, higher thermal conductivity. EFFECT: more short time processing with minimal expenditure of electric power. 2 cl