FIELD: liquid radiowastes immobilization in solid stable medium. SUBSTANCE: dry residue of sulphur-containing radiowastes is mixed up with vitrifying dopes; calcium fluoride in amount of 6-10 mass percent 3-10 mass percent of residue sulfate ions is introduced in mixture. Charge obtained is heated up to formation of glass melt whereupon the latter is cooled down in solid state. EFFECT: simplified procedure, improved water resistance of end product.
Title | Year | Author | Number |
---|---|---|---|
RADIOACTIVE WASTE RECOVERY METHOD | 1997 |
|
RU2108633C1 |
METHOD OF NEUTRALIZING RADIOACTIVE WASTE OF VARIABLE COMPOSITION | 0 |
|
SU1597936A1 |
METHOD FOR SOLIDIFYING RADIOACTIVE WASTE | 1995 |
|
RU2079911C1 |
METHOD FOR RADIOACTIVE WASTE FIXING ON INORGANIC MATERIAL MATRIX | 1991 |
|
RU2008733C1 |
METHOD AND DEVICE FOR VITRIFYING RADIOACTIVE ASH | 1998 |
|
RU2152652C1 |
METHOD OF PROCESSING MIXTURES OF CATION-EXCHANGE AND ANION-EXCHANGE RESINS CONTAINING RADIOACTIVE AND TOXIC ELEMENTS | 1998 |
|
RU2140107C1 |
METHOD OF VITRIFICATION OF LIQUID RADIOACTIVE WASTE | 0 |
|
SU1738006A1 |
PROCESS OF VITRIFICATION OF RADIOACTIVE AND TOXIC WASTE IN FURNACE | 1992 |
|
RU2035073C1 |
METHOD FOR PRODUCING STARTING MELT IN COLD-CRUCIBLE INDUCTION FURNACES DURING VITRIFICATION OF RADIOACTIVE WASTES | 1995 |
|
RU2091875C1 |
METHOD FOR EMBEDDING SODIUM NITRATE CONTAINING LIQUID RADIOACTIVE WASTES IN CERAMIC MATRIX | 1995 |
|
RU2086019C1 |
Authors
Dates
1996-08-10—Published
1993-07-26—Filed