FIELD: investigating materials. SUBSTANCE: stainless steel bearing under 13% chromium is kept in solution made up of (by g/l) MgCl2·6H2O 180-200 or NaCl 120-140, Na2S2O3 18-23, the balance water at a temperature of 60-65 C for 10 hours until cracks develop. EFFECT: reduced analysis duration, obviated necessity for using toxic substances. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TESTING SUSCEPTIBILITY OF HIGH-STRENGTH STAINLESS STEELS TO CORROSION CRACKING | 1992 |
|
RU2011184C1 |
HIGH STRENGTH-CORROSION RESISTANT OF AUSTENITE- MARTENSITE CLASS | 1999 |
|
RU2164546C2 |
COMPOSITION FOR REMOVING ATMOSPHERE CORROSION PRODUCTS FROM SURFACE OF STAINLESS STEEL | 1994 |
|
RU2105085C1 |
HIGH-STRENGTH CORROSION RESISTANT STEEL OF MARTENSITE TYPE | 1995 |
|
RU2077602C1 |
METHOD FOR MANUFACTURE OF SEMIFINISHED AND/OR FINISHED ARTICLES FROM ALUMINIUM-LITHIUM ALLOYS | 1994 |
|
RU2048592C1 |
STEEL RESISTANT TO CORROSION IN HYDROGEN SULPHIDE-CONTAINING ENVIRONMENTS OF OIL AND GAS FIELDS | 2022 |
|
RU2810411C1 |
METHOD OF PROTECTION OF STEEL MACHINE COMPONENTS FROM SALT ATTACK | 1999 |
|
RU2165475C2 |
ALUMINUM-BASED HIGH-STRENGTH ALLOY AND PRODUCT MANUFACTURED THEREFROM | 2000 |
|
RU2184166C2 |
METHOD FOR HEAT TREATMENT OF SEMIFINISHED PRODUCTS FROM DEFORMABLE ALUMINIUM-LITHIUM ALLOYS | 1994 |
|
RU2048591C1 |
REFRACTORY NICKEL-BASED ALLOY FOR MOLDED PIECES WITH DIRECTED AND MONOCRYSTALLINE STRUCTURE | 1995 |
|
RU2114206C1 |
Authors
Dates
1994-04-30—Published
1992-03-05—Filed