FIELD: metallurgy. SUBSTANCE: method involves heating for hardening and cooling at the rate of 0,5-3 Vcr, where Vcr critical cooling rate and two-stage cooling for ageing. EFFECT: higher failure viscosity, corrosion resistance, and reduced internal residual stresses at a high level of mechanical properties. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURE OF SEMIFINISHED AND/OR FINISHED ARTICLES FROM ALUMINIUM-LITHIUM ALLOYS | 1994 |
|
RU2048592C1 |
METHOD FOR PROCESSING OF HALF-FINISHED PRODUCTS OF ALLOY OF Al-Mg-Li-Sc SYSTEM | 1991 |
|
RU2031970C1 |
HIGH-STRENGTH ALUMINIUM-BASED ALLOY AND METHOD FOR OBTAINING ITEMS FROM IT | 2010 |
|
RU2443793C1 |
METHOD OF MANUFACTURING INTERMEDIATE PRODUCTS FROM ALUMINUM ALLOY, AND ARTICLE OBTAINED BY THIS METHOD | 2003 |
|
RU2238997C1 |
METHOD OF THERMOMECHANICAL TREATMENT OF SEMI-FINISHED PRODUCTS MADE FROM ALUMINUM ALLOYS | 2004 |
|
RU2256720C1 |
CORROSION-RESISTANT ALUMINUM-BASE ALLOY, METHOD OF PRODUCTION OF SEMIFINISHED PRODUCTS AND ARTICLE FOR THIS ALLOY | 1999 |
|
RU2163938C1 |
METHOD FOR THERMAL PROCESSING OF SEMI-FINISHED PRODUCTS AND ARTICLES OF ALUMINUM-BASE ALLOY | 2003 |
|
RU2235799C1 |
METHOD FOR HEAT TREATMENT OF SEMIFINISHED PRODUCTS AND ARTICLES OF ALUMINUM-BASE ALLOY | 2002 |
|
RU2235143C2 |
METHOD OF MAKING OF WELDED JOINT MADE OF ALLOYS OF SYSTEM ALUMINIUM- MAGNESIUM-LITHIUM | 1990 |
|
RU1762572C |
METHOD OF MANUFACTURING COMPRESSED INTERMEDIATE PRODUCTS FROM ALUMINUM ALLOY, AND PRODUCT OBTAINED THEREFROM | 2003 |
|
RU2238998C1 |
Authors
Dates
1995-11-20—Published
1994-04-27—Filed