FIELD: metallurgy. SUBSTANCE: silica is mixed with a reducing mixture having a moisture content of 25-40 wt % , the charge is loaded into the mouth of an ore thermal furnace and maintained for 3-10 min and then fed into the furnace and melted. EFFECT: improved properties of the silicon. 1 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SILICON PREPARING | 0 |
|
SU1791379A1 |
PROCESS FOR PREPARING CARBON REDUCING AGENT FOR MELTING SILICON | 1989 |
|
RU2032616C1 |
METHOD OF SILICON PRODUCING | 1991 |
|
RU2094372C1 |
METHOD OF TECHNOLOGICAL SILICON RECEIVING | 2007 |
|
RU2352524C1 |
BRIQUETTING MIXTURE FOR MANUFACTURING COMMERCIAL-GRADE SILICON AND PROCESS FOR PRODUCING SAME | 1992 |
|
RU2036144C1 |
METHOD OF CARBO-THERMAL REDUCTION OF SILICON | 2008 |
|
RU2383493C1 |
METHOD FOR PROCESSING OF ALKALINE ALUMINOSILICATE RAW MATERIALS | 1992 |
|
RU2060941C1 |
METHOD FOR SILICON PRODUCTION IN ELECTRIC ARC FURNACE | 1991 |
|
RU2038298C1 |
METHOD OF OBTAINING SILICON | 0 |
|
SU1535825A1 |
METHOD OF MELTING SILICON IN ORE-SMELTING FURNACE | 0 |
|
SU1701631A1 |
Authors
Dates
1994-05-30—Published
1991-06-03—Filed