FIELD: electrical engineering. SUBSTANCE: petroleum coke precalcined at a temperature of 1200 C for 12 minutes is reduced to a grain size of (-8 mm) and mixed with a 28-30 wt % liquid coal pitch, agglomerated and heat treated at 950 C for 50 minutes. The carbon reducing agent is pitch coke. EFFECT: improved properties of the carbon reducing agent. 2 cl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR MELTING SILICON | 1991 |
|
RU2013370C1 |
METHOD OF PREPARING ELECTRODE PASTE | 1997 |
|
RU2132411C1 |
METHOD FOR PRODUCTION OF ANODE MATERIAL | 1996 |
|
RU2116383C1 |
METHOD OF PREPARING BURDEN FOR SILICON MELTING | 1992 |
|
RU2042721C1 |
PROCESS OF PREPARATION OF COLD-RAMMED BOTTOM MASS FOR ALUMINUM ELECTROLYZERS | 1996 |
|
RU2128731C1 |
CHARGE FOR PRODUCTION OF SILICON AND METHOD OF PREPARING MOLDING MATERIAL FOR PRODUCTION OF SILICON | 1997 |
|
RU2151738C1 |
ELECTRODE PASTE FOR SELF-BAKING ELECTRODES IN ORE-REDUCING FURNACES AND METHOD OF PREPARING IT | 1997 |
|
RU2121989C1 |
CARBON-CONTAINING CHARGE FOR LARGE-SIZED GRAPHITIZED BLANKS | 1990 |
|
SU1790136A1 |
METHOD FOR PREPARING BURDER FOR MANUFACTURING SILICON | 0 |
|
SU1666443A1 |
METHOD OF PRODUCING ANODE MASS FOR SELF-BURNING ANODES IN ALUMINIUM ELECTROLYZERS | 1995 |
|
RU2091511C1 |
Authors
Dates
1995-04-10—Published
1989-04-20—Filed