FIELD: metallurgy. SUBSTANCE: method provides for use of new components, change components ratio during molten bath processing as in a ladle, as in a mold. Charge is loaded in furnace, bring the molten bath up to given temperature, exercise modification of metal by in series addition of modifying mixtures at the first stage - in a ladle, at the second stage - in a mold. Modification in the ladle is exercised by a mixture, that has compositions of refractory metals, inoculator, made as ultra-dispersed powder or its composition, and cryolite in amount of 0.020 - 0.095 % of molten metal weight. Modification in a mold is exercised by addition in a molten bath of mixture, that has coke and one or several components from group of calcium-silicon, ferrosilicon in amount of 0.15 - 0.45 kg/ton. Composition of refractory metals, inoculator are added in ratio of 100 : (1 - 10). Complex modification is exercised in a mold by coke addition together with calcium-silicon and/or ferrosilicon, taken in ration of 1 : (1 - 5). EFFECT: method provides for production of ingots good for processing with high strength, firmness and plasticity. 4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MODIFICATION OF CAST ALLOYS | 2012 |
|
RU2525967C2 |
PRODUCTION OF COMPACTED IRON MODIFIER BASED ON NANO-DISPERSED POWDERS | 2013 |
|
RU2522926C1 |
CAST IRON AND SILUMIN MODIFYING METHOD | 2010 |
|
RU2439166C2 |
METHOD FOR MODIFICATION OF ALUMINIUM ALLOYS | 1992 |
|
RU2016112C1 |
EXOTHERMIC MIXTURE | 0 |
|
SU1093711A1 |
MIX FOR MODIFYING GREY CAST IRON | 0 |
|
SU1079684A1 |
BRIQUETTED MIXTURE FOR INOCULATION OF GRAY IRON | 1997 |
|
RU2124566C1 |
METHOD FOR MAKING CAST IRON WITH DIFFERENT TYPE OF GRAPHITE | 2001 |
|
RU2181775C1 |
METHOD FOR PRODUCING MODIFIED GREY CAST IRON | 0 |
|
SU1097680A1 |
MODIFIER FOR IRON-CARBON MELTS AND METHOD FOR ITS MANUFACTURE | 2021 |
|
RU2776573C1 |