FIELD: metallurgy. SUBSTANCE: modifying mixture is added into melted charge, its quantity being 0.02-0.20 mass % of charge mass. Said mixture contains carbide- and nitride- forming elements and oxides of aluminium and copper at ratio 30-70:0.1-0.5 together with alkali and alkali-earth elements and with their compounds; ratio of aluminium and copper oxides being 100: 0.01-0.98. EFFECT: improves airtightness of casting, increases its strength and plasticity. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MODIFICATION OF CAST ALLOYS | 2012 |
|
RU2525967C2 |
IRON PRODUCTION METHOD | 1991 |
|
RU2016071C1 |
MIXTURE FOR MANUFACTURING REFRACTORY ARTICLES | 1996 |
|
RU2096386C1 |
MODIFIER FOR IRON-CARBON MELTS AND METHOD FOR ITS MANUFACTURE | 2021 |
|
RU2776573C1 |
MODIFIER FOR IRON-CARBON MELTS AND METHOD FOR ITS PRODUCTION | 2022 |
|
RU2779272C1 |
CASTING ALLOYING METHOD | 2015 |
|
RU2630990C2 |
REFRACTORY ALLOY | 1998 |
|
RU2149208C1 |
REFRACTORY ALLOY | 1998 |
|
RU2149203C1 |
REFRACTORY ALLOY | 1998 |
|
RU2149209C1 |
REFRACTORY ALLOY | 1998 |
|
RU2149204C1 |
Authors
Dates
1994-07-15—Published
1992-04-08—Filed