FIELD: machine engineering, aircraft building and other industry branches. SUBSTANCE: method comprises steps of heating a part with openings with use of annular electrodes up to 760 C and cooling it by rotating cone sprayer with pitch of the openings, being increased along the article; the liquid is being fed by a predetermined angle relative to the article surface. EFFECT: simplified strengthening process. 1 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF THERMOPLASTIC HARDENING OF PARTS AND PLANT FOR REALIZATION OF THIS METHOD | 2003 |
|
RU2258086C1 |
OPENING SURFACE HARDENING METHOD | 1991 |
|
RU2015180C1 |
METHOD FOR THERMOPLASTIC STRENGTHENING OF PARTS AND INSTALLATION FOR ITS REALISATION | 2006 |
|
RU2351660C2 |
METHOD OF QUENCHING SPRING TERMINALS AND PLANT TO THIS END | 2011 |
|
RU2459877C1 |
PROCEDURE FOR THERMO-PLASTIC REINFORCEMENT OF PARTS | 2009 |
|
RU2411303C1 |
PLANT FOR THERMAL PLASTIC HARDENING OF LARGE-SIZED ARTICLES | 2002 |
|
RU2219250C1 |
UNIT FOR THERMOPLASTIC STRENGTHENING OF ARTICLES | 0 |
|
SU730832A1 |
UNIT FOR THERMOPLASTIC STRENGTHENING OF BLADES | 0 |
|
SU726187A1 |
METHOD FOR RESTORING QUENCHED SLEEVES OF CYLINDERS | 2000 |
|
RU2181649C2 |
METHOD FOR RECOVERY OF INNER AND OUTER SURFACES OF CAST IRON CYLINDER CASINGS | 2000 |
|
RU2174901C1 |
Authors
Dates
1994-07-15—Published
1991-01-02—Filed