FIELD: metallurgy. SUBSTANCE: carbonaceous or carbon-containing fiber (diameter is 7-10 microns, length is 260-400 microns) is added at the mixing of coke with pitch at concentration 1.5-2.4% by mass. Carbon fiber must be impregnated with pitch preliminary. Properties of material prepared: values of bending, compression and expansion strength are 438, 900 and 275 kgs/cm2, respectively. EFFECT: improved method of reinforced graphite making. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FINE GRAIN GRAPHITE PRODUCTION | 1992 |
|
RU2069205C1 |
ELECTRIC BRUSH MANUFACTURING PROCESS | 1994 |
|
RU2088007C1 |
METHOD FOR PRODUCTION OF FINE-GRAINED GRAPHITIZED MATERIAL | 1991 |
|
RU2035395C1 |
METHOD OF CALCINING LARGE-SIZE CARBON BLANKS | 1989 |
|
RU2022921C1 |
METHOD OF CARBON FIBROUS MATERIAL PREPARING | 1991 |
|
RU2016146C1 |
METHOD OF PRODUCING FINE-GRAINED LARGE-SIZED GRAPHITIZED BILLETS | 0 |
|
SU1834843A3 |
CHARGE FOR CARBON-GRAPHITE ARTICLES (MAINLY CRYSTALLIZERS) PRODUCTION | 1991 |
|
RU2009998C1 |
METHOD FOR MANUFACTURE OF BLANKS USED FOR PRODUCTION OF GRAPHITE MATERIAL | 1991 |
|
RU2036136C1 |
METHOD OF MANUFACTURING CONSTRUCTIONAL HEAT-INSULATION CARBON MATERIAL AND CONSTRUCTIONAL HEAT-INSULATION CARBON MATERIAL | 1992 |
|
RU2093494C1 |
METHOD OF CONTROLLING PROCESS OF PRODUCING CARBON PRODUCTS | 1992 |
|
RU2085485C1 |
Authors
Dates
1994-07-30—Published
1991-02-26—Filed