FIELD: inorganic chemistry. SUBSTANCE: molybdenum trioxide is subjected to mechanical-chemical activation. The activated molybdenum trioxide is dissolved in phosphoric acid. The Mo-to-P molar ratio is 9. The temperature is 40-100 C. The MoO3 concentration in the solution is not higher than 10 wt % . The solution is kept at a temperature of 0-25 C for at least 20 days. EFFECT: improved process.
Title | Year | Author | Number |
---|---|---|---|
CATALYST FOR PREPARING 2,3:4,6-DIISOPPROPYLIDENE-ALPHA-L- -SORBOFURANOSE AND PROCESS FOR PREPARING THE SAME | 1995 |
|
RU2080923C1 |
METHOD OF PREPARING PHOSPHORUS HETEROPOLYACIDS | 1994 |
|
RU2076070C1 |
PROCESS FOR PREPARING HETEROPOLYACIDS | 1992 |
|
RU2076071C1 |
METHOD FOR PREPARING 12-PHOSPHOROTUNGSTIC ACID | 1988 |
|
RU1559773C |
CATALYST FOR OXIDATION OF CARBON MONOXIDE AND METHOD OF PREPARING THE SAME | 1983 |
|
SU1135054A1 |
CATALYST FOR LOW-TEMPERATURE OXIDATION OF CARBON OXIDE | 1989 |
|
RU1684997C |
METHOD FOR PURIFICATION OF POLYESTERS | 1991 |
|
RU2050377C1 |
PROCESS FOR PREPARING 2-METHYL-1,4-NAPHTHAQUINONE | 1992 |
|
RU2061669C1 |
0 |
|
SU1782934A1 | |
METHOD OF PREPARING CATALYZER FOR LIQUID-PHASE OXIDIZING OF OLEFIN C- C IN KETONE | 1981 |
|
SU1031045A1 |
Authors
Dates
1994-09-15—Published
1992-04-10—Filed