FIELD: test equipment. SUBSTANCE: method consists in production of specimen, bringing-on of stress concentrator and crack and subsequent test up to breaking, stress concentrator and crack are made by edge welding of two preliminarily grooved, polished plates contacting on chamfered polished surfaces, compressed by distributed load selected from condition δ<0,25δy, where δ - compression stresses on plate chamfered surfaces, dy - yield point. EFFECT: enhanced accuracy of estimation of base metal breaking toughness. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DETERMINATION OF TOUGHNESS FACTOR OF BASE METAL BREAKING IN WELD AREA | 1991 |
|
RU2019808C1 |
PROCEDURE FOR REPAIR OF STEEL STRUCTURES BY WELDING | 2009 |
|
RU2400342C1 |
METHOD TO CHECK PIPES FOR ANTIRUST STRENGTH | 2008 |
|
RU2368888C1 |
METHOD FOR EVALUATING RESISTANCE OF ALLOYS TO FORMATION OF HOT CRACKS DURING WELDING | 1991 |
|
RU2016727C1 |
METHOD OF MAKING WELDED COMPOSITE COLUMN TYPE SAMPLE FOR TESTING CRACK RESISTANCE OF IRRADIATED METAL | 2015 |
|
RU2582626C1 |
0 |
|
SU114865A1 | |
METHOD OF REPAIRING MAIN PIPELINES | 2004 |
|
RU2277667C1 |
IMPROVED METHOD FOR CYCLIC TESTING OF FULL-THICKNESS SAMPLES OF MAIN PIPELINES FOR STRESS CORROSION CRACKING | 2023 |
|
RU2820157C1 |
METHOD OF CRACKED PIPE LAPPED JOINT/PATCH STRENGTH TEST | 0 |
|
SU1665279A2 |
SPECIMEN FOR TESTING WELDED JOINT FOR CORROSION CRACKING | 0 |
|
SU1244572A1 |