FIELD: refractory linings of converters. SUBSTANCE: gunning mixture contains 50-90 % by weight of refractory material, 2-30 % by weight of carbon-containing constituent and 2-30 % by weight of hot constituent. The hot constituent includes aluminum as the alloy containing 1-99 % by weight of Mg, or the powdered mixtures of aluminum comprising 0.5-50 % by weight of Mg. EFFECT: decrease in specific consumption of refractory material. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
REFRACTORY MIXTURE | 2007 |
|
RU2379255C2 |
SPINEL-PERICLASOCARBON REFRACTORY | 1997 |
|
RU2167123C2 |
REFRACTORY MIXTURE | 2010 |
|
RU2445290C1 |
SPINEL-CONTAINING REFRACTORY MATERIAL WITH CARBON BINDER | 1998 |
|
RU2130440C1 |
CARBON-CONTAINING REFRACTORY MATERIAL | 1997 |
|
RU2108311C1 |
FIRE-RESISTANT GUN MIXTURE | 2010 |
|
RU2424213C1 |
METHOD OF REFRACTORY COATING PREPARING ON THE HOT SURFACE AND POWDERY MIXTURE FOR REFRACTORY COATING PREPARING | 1990 |
|
RU2027690C1 |
PERICLASE-SPINEL REFRACTORY PRODUCTS AND A METHOD FOR MANUFACTURE THEREOF | 2002 |
|
RU2235701C1 |
METHOD OF PRODUCING PERICLASE-CARBON CONCRETE AND PERICLASE-CARBON CONCRETE | 2023 |
|
RU2818338C1 |
CARBON- CONTAINING REFRACTORY | 2000 |
|
RU2163900C1 |
Authors
Dates
1994-11-15—Published
1990-04-25—Filed