FIELD: heat-exchange parts. SUBSTANCE: method includes application of adhesive selected from conditions of full burning out in sintering. Spray-coated on adhesive before its drying is powder material with melting temperature equalling 0.65-0.95 of melting temperature of material of previous layer, and produced layer is subjected to sintering. EFFECT: higher efficiency.
Title | Year | Author | Number |
---|---|---|---|
APPARATUS FOR POWDER MATERIALS COVER APPLICATION ON INNER SURFACES OF LENGTHENED PIPES | 1992 |
|
RU2015854C1 |
METHOD OF PREPARING WATER-OXIDE BINDING SUSPENSION | 1996 |
|
RU2118627C1 |
METHOD OF MANUFACTURING CERAMIC FILTER ELEMENT | 2001 |
|
RU2204542C1 |
MATERIAL FOR GAS-THERMAL APPLICATION, METHOD OF ITS MANUFACTURE AND METHOD OF ITS APPLICATION | 2016 |
|
RU2646299C2 |
METHOD FOR TREATING INTERNAL SURFACES OF BAKING MOLDS | 1991 |
|
RU2025977C1 |
METHOD FOR MAKING NANOSTRUCTURED FUNCTIONAL-GRADIENT WEAR-RESISTANT COATING | 2007 |
|
RU2354749C2 |
METHOD FOR ANTICORROSION PROTECTION OF METAL SURFACES | 1994 |
|
RU2084480C1 |
METHOD FOR PRODUCING THREE-DIMENSIONAL METALLIC ARTICLES AND APPARATUS FOR PERFORMING THE SAME | 2003 |
|
RU2288073C2 |
METHOD OF FORMING THERMAL BARRIER COATING | 2003 |
|
RU2325467C2 |
METHOD OF APPLYING NANOSTRUCTURISED WEAR-RESISTANT ELECTROCONDUCTIVE COVERINGS | 2007 |
|
RU2362839C1 |
Authors
Dates
1995-01-27—Published
1992-02-18—Filed