FIELD: medical equipment. SUBSTANCE: rubber mix contains: mas.part.: ethylene-propylene rubber 100; chlorosulfonated polyethylene 12-16; sulfur vulcanizing group 6.7- 6.8 and X-ray protective filler in form of optical polishing powder containing cerium dioxide at least 70 mas.% and 9-14% of fluorine-ion 476-695. Material characteristics: lead equivalent for sample thickness δ corresponding to 0.6 mm of Pb is 2.47-2.58 mm; tensile strength 45-48 kgf/sq.cm; elongation 145-160%; material is nontoxic, leaves no traces in touching, does not crumble in prolonged service on bends and preserves its monolithic structure. EFFECT: higher efficiency. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
RUBBER MIXTURE FOR MANUFACTURING OF RUBBER BEING PROTECTION AGAINST X-RAYS | 1992 |
|
RU2054439C1 |
ELECTRICALLY INSULATING MATERIAL PREPARATION METHOD | 2017 |
|
RU2644896C1 |
ELECTRIC CABLE | 1980 |
|
RU1090170C |
THERMORADIATION-RESISTANT ELASTOMER COMPOSITION | 2019 |
|
RU2709596C1 |
THERMOPLASTIC ELASTOMERIC MATERIAL | 2006 |
|
RU2334769C2 |
LAYERED RADIATION PROTECTIVE MATERIAL | 2016 |
|
RU2681520C2 |
POLYMERIC COMPOSITION FOR FILM COATING | 1990 |
|
RU2022979C1 |
WATER-SWELLABLE ELASTOMERIC COMPOSITION | 2020 |
|
RU2744283C1 |
LIGHT-WEIGHT RUBBER-POLYMER MATERIAL FOR MANUFACTURING PROTECTIVE CLOTHES AND METHOD OF OBTAINING THEREOF | 2013 |
|
RU2540976C2 |
AQUEOUS ADHESIVE FOR GLUING ELASTOMERS | 1994 |
|
RU2145623C1 |
Authors
Dates
1995-02-09—Published
1991-12-11—Filed