FIELD: glass making. SUBSTANCE: method includes glass smelt feed to forming aggregates includes smelt taking from a feeder and its feed to forming. Before feed to forming the smelt is brought to final viscosity, smelt cooling is decreased with shielding by cone housing-shunt from lining slag layer of hardened glass when producing glass fiber or from environment when producing glass balls. Then the smelt is fed to forming aggregates accounted for 1.05 to 1.2 of their given productivity. The smelt is brought up to final viscosity within 24 - 14; 150 - 80 Pa х s depending on glass chemical composition. EFFECT: glass of high quality. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ONE-STAGE PRODUCTION OF GLASS FIBERS | 1992 |
|
RU2031866C1 |
GLASS MELT FEEDING DEVICE | 1992 |
|
RU2029740C1 |
PROCESS FOR PREPARING FIBER GLASS | 1991 |
|
RU2013387C1 |
SPINNERET FEEDER TO EXTRUDE GLASS FIBRES BY ONE STAGE METHOD | 1992 |
|
RU2031867C1 |
FLOW FEEDER REPLACEMENT METHOD | 1992 |
|
RU2029741C1 |
DEVICE FOR DISMANTLING BURNT STREAM FEEDER | 1992 |
|
RU2029744C1 |
APPARATUS FOR PRODUCING FIBER FROM THERMOSTATIC MATERIAL | 0 |
|
SU1058905A1 |
METHOD OF PRODUCING HIGH-TEMPERATURE RESISTANT SILICA FIBER | 2020 |
|
RU2737438C1 |
GLASS FIBER PRODUCTION PLANT | 2001 |
|
RU2181346C1 |
GLASS-FORMING DEVICE FOR PRODUCTION OF GLASS FIBER | 1994 |
|
RU2064902C1 |
Authors
Dates
1995-02-27—Published
1992-06-01—Filed