FIELD: leather industry. SUBSTANCE: titanated semifinished product is treated with basic zirconium sulfate of the formula Zr(OH)y(SO4)x·nH2O where x = 0.6-0.8; y = 4-2x; n = 1-10 at ammonium sulfate consumption taken at 0.5-5% of depilated hide mass. EFFECT: improved method of leather output. 2 tbl