FIELD: processing of splits. SUBSTANCE: after preliminary washing and softening lower split is treated at 28-30 C by acid and salt, expense of acid being 1.5-2.0 % of split mass. Then tanning with the help of chromium compounds is carried out, expense of said compounds being 0.8-1.2 % of split mass as calculated for chromium oxide. Additional tanning is carried out using mentioned above chromium compounds together with carboxyl-containing polymers, expense of said reagents being 0.3-10 % of plained split as calculated for its dry residue. EFFECT: improves efficiency of the method. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR ELASTIC LEATHERS PRODUCTION | 0 |
|
SU1730172A1 |
| METHOD OF MANUFACTURING VELOURS FROM SPLIT | 2003 |
|
RU2225449C1 |
| METHOD FOR TREATMENT OF LEATHER | 1993 |
|
RU2039086C1 |
| 0 |
|
SU561733A1 | |
| METHOD OF LEATHER PRODUCTION FOR SHOES UPPER PART FROM THE SPLIT | 1993 |
|
RU2039834C1 |
| PROCESS FOR FINISHING LEATHER | 1993 |
|
RU2043421C1 |
| PROCESS FOR MAKING TANNED PELT | 1991 |
|
RU2005792C1 |
| CORIUM OF GENUINE LEATHER AND FUR SEMIFINISHED PRODUCT AND METHODS FOR MANUFACTURE THEREOF | 2002 |
|
RU2206620C1 |
| METHOD OF VELOUR PRODUCTION FROM THE SPLIT | 1993 |
|
RU2039836C1 |
| PROCESS FOR FINISHING LEATHER | 1993 |
|
RU2043420C1 |
Authors
Dates
1995-06-09—Published
1992-12-16—Filed