FIELD: treatment of leather. SUBSTANCE: decalcified and softened depilated hide is treated by glyoxal within 4-8 h. The process is carried out at pH 7-8 and at 30-40 C, quantity of glyoxal being 2-6 EFFECT: improves efficiency of the method. 1 tbl