FIELD: electrical engineering. SUBSTANCE: iron powder is compressed, pieces obtained are sintered, cooled down to 800-900 C and alloyed at this temperature by powdered silicon for 1-3 h. EFFECT: facilitated procedure. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING MAGNETICALLY-SOFT MATERIAL ON THE BASE OF FERRUM | 0 |
|
SU714518A1 |
METHOD OF NON-RETENTIVE MATERIAL RECEIVING | 2007 |
|
RU2350676C2 |
PROCEDURE FOR PRODUCTION OF MAGNETIC SOFT MATERIAL | 2009 |
|
RU2413320C1 |
METHOD OF PRODUCING NANOCOMPOSITE MATERIAL BASED ON COPPER, HARDENED BY CARBON NANOFIBRES | 2018 |
|
RU2696113C1 |
METHOD FOR OBTAINING MAGNETICALLY SOFT MATERIAL FOR MAGNETIC CONDUCTORS OF RELAYS | 2013 |
|
RU2553134C2 |
METHOD FOR OBTAINING SOFT MAGNETIC MATERIAL | 2013 |
|
RU2547378C2 |
SMELTED MAGNETIC MEDIUM ON BASIS OF SOFT MAGNETIC ALLOY AND MANUFACTURING METHOD FROM IT OF MONOLITHIC MAGNETIC CORE OF ELECTRICAL MACHINES | 2008 |
|
RU2376669C2 |
METHOD OF PRODUCING IRON-BASED PHOSPHORUS-BEARING POWDER | 2012 |
|
RU2494836C1 |
FERRUM POWDER BASED FERROMAGNETIC MATERIAL TO PRODUCE D,C, AND A,C, MAGNETIC CONDUCTORS | 0 |
|
SU1836731A3 |
METHOD OF PRODUCING LAMINATED MAGNETICALLY SOFT MATERIAL | 0 |
|
SU1517067A1 |
Authors
Dates
1995-03-10—Published
1991-01-30—Filed