FIELD: glass industry. SUBSTANCE: charge has silicate-containing component 20-50% ; alkaline-containing component 7-15%, and neutralized slime of galvanic manufacture - the rest. Charge can contain sand, blast furnace slag, oil shale ash or their mixture as a silicate-containing component. As an alkaline-containing component charge can contain soda or alkaline melt. Charge has the following composition, wt.-%: sand 20-30; soda 8-12; slime of galvanic manufacture - the rest, or sand 10-20; blast furnace slag 10-30; slime - the rest, or sand 10-20; blast furnace slag 10-30; alkaline melt 9-14; slime - the rest, or sand 10-20; oil shale ash 10-30; alkaline melt 8-11, and slime - the rest. Glass thermostability is 60-80 C. EFFECT: enhanced quality of charge. 7 cl, 4 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR UTILIZING OF SEWAGE PRECIPITATES OF ELECTROPLATING PROCESSES | 1994 |
|
RU2109699C1 |
METHOD OF PRODUCING GLASSCERAMIC MATERIAL | 2009 |
|
RU2424201C2 |
FIRE-RESISTANT VISCOUS-FLOW COMPOSITION | 2003 |
|
RU2255069C1 |
CHARGE FOR METALLURGICAL COKE PRODUCTION | 2015 |
|
RU2613501C1 |
CONCRETE MIX WITH IMPROVED CHARACTERISTICS WITH USE OF ELECTRIC FILTER SHALE ASH | 2014 |
|
RU2569701C1 |
MIXTURE FOR PREPARING QUENCHED CULLET FOR PRODUCING FOAMED GLASS-CERAMIC MATERIALS | 2009 |
|
RU2415817C1 |
CHARGE FOR OBTAINING GLASS | 2012 |
|
RU2494982C1 |
METHOD OF OBTAINING GRANULAR HEAT INSULATING MATERIAL | 2009 |
|
RU2403230C1 |
MIXTURE FOR OBTAINING CONSTRUCTION MATERIAL | 2011 |
|
RU2490224C1 |
CHARGE AND GLASS COMPOSITION FOR GLASS-CRYSTAL MATERIAL | 2021 |
|
RU2781058C1 |
Authors
Dates
1995-03-27—Published
1992-07-02—Filed