FIELD: processing of natural materials. SUBSTANCE: natural clay material is mixed with neutral aluminum salt and sodium hydroxide and at the same time, aluminum hydroxide is introduced in mixture. Then, mixture is subjected to steam heat treatment, and after subsequent thermal activation, it is mixed with aluminosilicate hydrogel to obtain homogeneous mass. Neutral aluminum salt is used in form of aluminum sulfate. Initial clay material is mixed with neutral aluminum salt and sodium hydroxide at mass ratio of 100: 0.05: 0.02, respectively. Steam heat treatment is carried out at temperature of 100-250 C for 10-60 min. EFFECT: higher efficiency. 3 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF GRANULATED ZEOLITE OF FAUJASITE TYPE BASED ON NATURAL CLAY MATERIALS | 1992 |
|
RU2033966C1 |
METHOD OF PREPARING GRANULAR FAUJASITE TYPE ZEOLITE WITHOUT BINDING MATERIALS | 1999 |
|
RU2174951C2 |
METHOD OF PRODUCTION OF SYNTHETIC ZEOLITE, TYPE A | 1999 |
|
RU2146222C1 |
METHOD OF SYNTHETIC FAUJASITE PRODUCING | 1997 |
|
RU2119453C1 |
METHOD OF PRODUCTION OF SYNTHETIC GRANULATED FAUJASITE | 1999 |
|
RU2146223C1 |
METHOD OF PREPARING HIGH PHASE-PURITY GRANULATED A-TYPE ZEOLITE | 2005 |
|
RU2283281C1 |
METHOD OF PREPARING SYNTHETIC A-TYPE ZEOLITE | 2005 |
|
RU2283280C1 |
METHOD OF PREPARING GRANULATED ZEOLITE ADSORBENT WITH HIGH PHASE-PURITY STRUCTURES A AND X | 2005 |
|
RU2283278C1 |
ZEOLITE X PRODUCTION METHOD | 1998 |
|
RU2142412C1 |
METHOD OF PREPARING GRANULATED HIGH-PHASE PURITY A AND X-STRUCTURE ZEOLITE ADSORBENT | 2001 |
|
RU2203220C1 |
Authors
Dates
1995-04-30—Published
1992-12-30—Filed