FIELD: ceramics. SUBSTANCE: charge for preparing of porous material containing aluminium oxide has a powder mixture of silicon carbide and one of oxides from the order: CaO, MgO, MnO, NiO, ZnO at the ratio SiC:MeO = 2: 1 at the following ratio of components, wt.-%: Al2O3 95-99; powder mixture of SiC and one of oxides from the order: CaO, MgO, MnO, NiO, ZnO (at ratio SiC: MeO = 2:1) 1-5. Proposed charge composition provides preparing of porous, strength and thermostable ceramics. Article strength is 25-45%, bending strength is 85-150 MPa, thermal stability is more then 30 heat changes at thermoshocks 1200 C - water. EFFECT: increased strength and thermal stability of material. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR PREPARING OF POROUS THERMOSTABLE CERAMIC MATERIAL | 1992 |
|
RU2031886C1 |
BATCH COMPOSITION FOR PRODUCTION OF DISCRETE CERAMIC MATERIALS FROM ZIRCONIA | 2002 |
|
RU2249570C2 |
METHOD FOR MANUFACTURING REFRACTORY LARGE-PORE TUBES | 2006 |
|
RU2318633C1 |
MIXTURE OF CERAMIC MATERIAL FOR HIGH-TEMPERATURE USE IN OXIDATIVE MEDIA | 2012 |
|
RU2498963C1 |
COMPOSITION FOR MANUFACTURING CERAMIC MATERIALS | 1996 |
|
RU2116278C1 |
COMPOSITE CERAMIC MATERIAL IN SiC-AlO SYSTEM FOR HIGH-TEMPERATURE USE IN OXIDATIVE MEDIA | 2012 |
|
RU2498957C1 |
COMPOSITION FOR CERAMIC MATERIAL MAKING | 1996 |
|
RU2100316C1 |
COMPOSITION OF CHARGE FOR HIGH-POROUS CELLULAR- STRUCTURE MATERIAL FOR CATALYST CARRIERS | 2002 |
|
RU2233700C2 |
CHARGE FOR MANUFACTURING OF IMPACT-RESISTANT CERAMICS (VERSIONS) | 2012 |
|
RU2514068C1 |
MIXTURE FOR MAKING POROUS PERMEABLE CERAMIC MATERIAL | 2008 |
|
RU2374208C1 |
Authors
Dates
1995-04-30—Published
1992-01-31—Filed