FIELD: glass industry. SUBSTANCE: charge has, wt.-%: boric acid (H3BO3) 12.12-36.36; potassium bichromate (K2Cr2O7) 4.24-11.09; lithium carbonate (Li2CO3) 12.73-18.74; lead oxide (PbO) 14.00-23.86, and silicic acid (SiO2·nH2O) -the rest. Charge has additionally, wt.-%: cobalt oxide (Co3O4) 0.29-2.39 and titanium oxide (TiO2) 0.17-0.55, and sum of these components is 1.38-2.37; additionally - cobalt oxide 0.15-0.28 and copper oxide (CuO) 0.78-0.91, and their sum is 0.93-2.19; additionally - cobalt oxide 0.92-1.72 and copper sulfate (CuSO4) 0.18-0.24, and their sum is 1.16-1.90; additionally - ferrochrome cupola slag 13.51-20.0. Charge components were mixed. Glass is founded at 1000-1050 C for 1-2 h, annealed at 450-470 C for 0.5 h. EFFECT: improved method of glass making. 6 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
SOLUTION FOR MAKING OF HOLLOW GLASS MICROSHERE | 1992 |
|
RU2033978C1 |
SOLUTION FOR MANUFACTURING HOLLOW GLASS MICROSPHERES | 1992 |
|
RU2036856C1 |
SOLUTION FOR MANUFACTURING HOLLOW GLASS MICROSPHERES | 1992 |
|
RU2036171C1 |
SOLUTION FOR PREPARING GLASS MICROSPHERE | 2001 |
|
RU2205802C2 |
AVENTURINE GLASS | 1991 |
|
RU2020135C1 |
AVANTURINE GLASS | 2001 |
|
RU2212380C2 |
METHOD OF MANUFACTURING GLASS MICROSPHERES WITH CONTROLLED PROPERTIES FROM SYNTHETIC BLENDS | 2001 |
|
RU2235693C2 |
GLASS FOR JEWELRY ENAMEL | 1992 |
|
RU2081071C1 |
THERMOSENSITIVE GLASS | 1993 |
|
RU2098365C1 |
ELECTROVACUUM GLASS | 1995 |
|
RU2108987C1 |
Authors
Dates
1995-05-20—Published
1993-01-27—Filed