FIELD: magnetic circuit manufacture. SUBSTANCE: method involves mixing of iron powder (90- 94 mass percent) and ferrophosphorus powder (6-10 mass percent) with phosphor content of 10-13 mass percent, their compaction and sintering in nitrogen atmosphere. EFFECT: reduced energy requirement due to lower cost of sintering atmosphere, improved safety in sintering, improved magnetic characteristics of nonretentive material obtained. 2 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PRODUCTION OF MAGNETIC SOFT MATERIAL | 2009 |
|
RU2413320C1 |
METHOD OF PRODUCTION OF MAGNETICALLY SOFT MATERIAL | 2005 |
|
RU2296382C1 |
METHOD FOR OBTAINING MAGNETICALLY SOFT MATERIAL FOR MAGNETIC CONDUCTORS OF RELAYS | 2013 |
|
RU2553134C2 |
METHOD FOR OBTAINING SOFT MAGNETIC MATERIAL | 2013 |
|
RU2547378C2 |
METHOD OF NON-RETENTIVE MATERIAL RECEIVING | 2007 |
|
RU2350676C2 |
SINTERED MAGNET AND METHODS OF ITS OBTAINING | 2013 |
|
RU2629124C9 |
POWDERED METAL COMPOSITION FOR EASY PROCESSING BY CUTTING | 2017 |
|
RU2735532C2 |
CHARGE FOR PREPARING STRUCTURAL CAKED MATERIAL | 1992 |
|
RU2031177C1 |
METHOD OF IRON POWDER PRODUCTION | 2013 |
|
RU2529129C1 |
METHOD OF MANUFACTURING PHOSPHORUS STEEL | 1998 |
|
RU2132254C1 |
Authors
Dates
1995-07-25—Published
1992-08-27—Filed