FIELD: building industry. SUBSTANCE: concrete mixture has, wt.-%: portland cement 18.9-19.4; rubble 44.1-44.5; sand 35.0-35.6; superplasticizer based on naphthalene-sulfoacid sodium salt with formaldehyde C-3 0.1-62; powder-like polyvinyl acetate 0.8-1.1; methylpyrazole 0.1-0.2. Compression strength of concrete is 37.5 MPa, water absorption is 3.15%; density is 2.29 t/m3; adhesion to metal is 12.6 MPa; adhesion to concrete is 14.3 MPa; current density at E = 1500 mv mcA/cm2 after 30 test cycles is about 3.2. EFFECT: enhanced quality of mixture. 2 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| CONCRETE MIX | 1992 | 
 | RU2057098C1 | 
| CONCRETE MIX AND METHOD OF ITS PREPARATION | 1998 | 
 | RU2131856C1 | 
| GLASS-FIBER-CONCRETE MIXTURE | 1990 | 
 | SU1811681A1 | 
| DRY MIXTURE FOR STEEL FITTINGS PROTECTION AGAINST CORROSION | 1993 | 
 | RU2064908C1 | 
| COMPLEX ADDITION FOR CONCRETE MIXTURE | 1992 | 
 | RU2041863C1 | 
| CONCRETE MIXTURE | 2017 | 
 | RU2668600C1 | 
| METHOD OF CONCRETE MIXTURE PREPARING | 1991 | 
 | RU2016885C1 | 
| SEAMLESS POURED-IN-PLACE CONCRETE FLOOR | 1998 | 
 | RU2137730C1 | 
| DRY MORTAR MIXTURE | 2002 | 
 | RU2214376C1 | 
| METHOD OF MANUFACTURING HIGH-STRENGTH CELLULAR CONCRETE | 1998 | 
 | RU2133722C1 | 
Authors
Dates
1996-08-10—Published
1993-12-09—Filed