FIELD: fireproof foil glass-plastics production. SUBSTANCE: composition has, mas. p. epoxy diane resin 100; mixture of 4,4'-diaminediphenylmethan and 4,4'-diaminediphenylsulfone at the ratio (1:2)-(1:3) 8.8-16.5; arsenic glycolate (+3) in the form of 40-90% solution in ethylene glycol or acetone, toluene, ethylcellosolve, dioxane 5.2-50.0; organic solvent 125-195. EFFECT: enhanced quality of binder composition. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDER COMPOSITION FOR LAYERED INSULATING MATERIAL | 1994 |
|
RU2047627C1 |
PROCESS FOR TREATING ARSENIC-CONTAINING WASTE | 1992 |
|
RU2041879C1 |
METHOD OF PREPARING BROMO-CONTAINING EPOXY RESIN FOR FIRE-RESISTANT FLAKY PLASTICS | 1992 |
|
RU2041888C1 |
INSULATION COMPOUND PREPARATION METHOD | 2003 |
|
RU2247752C1 |
EPOXY BINDER FOR REINFORCED PLASTIC | 2012 |
|
RU2505568C1 |
POLYMER BINDER FOR REINFORCED PLASTIC | 2006 |
|
RU2323236C1 |
EPOXY BINDING AGENT FOR PREPREGS, PREPREG BASED ON IT, AND ARTICLE MADE THEREOF | 2006 |
|
RU2335515C1 |
METHOD FOR PRODUCING UNCOMBUSTIBLE FOIL-FACED HETINAX | 0 |
|
SU1666361A1 |
EPOXIDE GLUE COMPOSITION, PREPREG BASED THEREON, AND PRODUCT MANUFACTURED THEREFROM | 2003 |
|
RU2230764C1 |
ADHESION COMPOSITION | 1992 |
|
RU2039784C1 |
Authors
Dates
1995-08-20—Published
1993-03-11—Filed