FIELD: inorganic chemistry. SUBSTANCE: titanium dioxide being heated preliminary to 120-250 C is treated with the help of wetted air. Expense of said air is 0,17-0,35 m3/kg, its temperature being 300-500 C. Air may be fed as mixture with steam of surface active substance (e.g. organic alcohol or amine), its quantity being 0.1-0.3 of titanium dioxide. During said treatment gaseous dispersion of titanium dioxide is affected by ultraviolet irradiation. EFFECT: improves efficiency of the method. 4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
TITANIUM DIOXIDE PIGMENT MANUFACTURE METHOD (OPTIONS) | 2003 |
|
RU2236376C1 |
METHOD OF MODIFYING PIGMENT TITANIUM DIOXIDE | 1993 |
|
RU2042693C1 |
METHOD OF SUPERFICIAL PROCESSION OF PIGMENT TITANIUM DIOXIDE | 2006 |
|
RU2333923C1 |
0 |
|
SU430134A1 | |
METHOD OF PREPARING THE REAGENT FOR WATER TREATMENT | 1993 |
|
RU2087425C1 |
COMPOSITION FOR TREATMENT OF NATURAL WATER AND WASTE WATERS AND A METHOD FOR PREPARING COMPOSITION FOR TREATMENT OF NATURAL AND WASTE WATERS | 2000 |
|
RU2179954C1 |
REACTOR FOR CONDUCTING PROCESS OF TITANIUM DIOXIDE DECHLORINATION | 2002 |
|
RU2223916C1 |
METHOD OF PRODUCING FILTERING-SORBING MATERIAL WITH PHOTO CATALYTIC PROPERTIES | 2011 |
|
RU2482912C1 |
PIGMENT TITANIUM DIOXIDE PRODUCTION METHOD | 1998 |
|
RU2125018C1 |
PROCESS FOR DESMERCURIZATION OF SURFACES | 0 |
|
SU1678878A1 |
Authors
Dates
1995-08-27—Published
1993-06-29—Filed