FIELD: production of concrete mixes. SUBSTANCE: method involves preliminary processing of 3.45-46.15 wt.-% of cement jointly with superplasticizer introduced in the amount of 2.5-20% of the mass of cement, under a mechanical action of 30-120 W per kilogram of the treated mix within 20-3,6·104 s followed by mixing with the remaining cement, fillers, and water. Power expenditures for treatment of 1 m3 of concrete mix are reduced, the plasticizer consumption diminishes by 53.85-96.55 wt.-% with unchanged strength of concrete and the total cement consumption. EFFECT: reduced consumption of superplasticizer and power expenditures while retaining the same strength of concrete and consumption of cement. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
SUPERPLASTICIZER | 1989 |
|
SU1676209A1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2009 |
|
RU2399597C1 |
METHOD FOR PREPARATION OF CONCRETE MIX | 1986 |
|
SU1812769A1 |
METHOD AND PROCESS LINE FOR MANUFACTURING ESPECIALLY-HIGH-STRENGTH CEMENT CONCRETE | 1997 |
|
RU2106327C1 |
METHOD OF PREPARING CONCRETE MIXTURE FOR HIGH-STRENGTH CONCRETE | 2020 |
|
RU2739006C1 |
METHOD FOR PREPARING CONCRETE MIXTURE | 2016 |
|
RU2617818C1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2009 |
|
RU2391307C1 |
METHOD OF PREPARATION OF CONCRETE "FLINT STONE -GRANITE" | 2006 |
|
RU2348598C2 |
METHOD TO PREPARE CONCRETE MIXTURE | 2010 |
|
RU2443650C1 |
FILLING MIXTURE COMPOSITION | 2010 |
|
RU2433274C1 |
Authors
Dates
1995-08-27—Published
1987-04-09—Filed