FIELD: chemistry.
SUBSTANCE: invention relates to the technology of preparing concrete mixtures, mainly for high-strength concrete, used for making articles and structures used in industrial and civil construction when erecting special-purpose structures. Method involves mixing cement, sand, crushed stone, additives and water. At that, at first, into the mixer is loaded and mixed to obtain a homogeneous mixture of 5–20 mm fractioned grains, ordinary quartz sand with a fineness modulus of not less than 2.1, lignosulphonate additive ST 1.4 in amount of dry substance 0.1–0.15 % of consumption cement and 70–80 % of tempering water. After that, cement, polycarboxylate base-based superplasticizer ST 5.0 in amount of 0.30–0.35 % of dry matter of cement consumption, as well as the rest of the tempering water are added to the obtained mixture and all components are finally mixed until a homogeneous concrete mixture is obtained.
EFFECT: technical result is higher mobility of concrete mixture without reducing strength of concrete in 28-day age of normal hardening.
1 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPLEX CONCRETE MIXTURE ADDITIVE | 2022 |
|
RU2795636C1 |
CRUDE MIXTURE FOR HIGH-STRENGTH CONCRETE | 2011 |
|
RU2466110C1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2019 |
|
RU2730235C1 |
HIGH-STRENGTH CONCRETE | 2010 |
|
RU2433099C1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2019 |
|
RU2714895C1 |
METHODS OF INCREASING CONCRETE STRENGTH AT COMPRESSION USING NANOSILICA OBTAINED FROM HYDROTHERMAL SOLUTION | 2015 |
|
RU2599739C1 |
HIGH-STRENGTH CONCRETE | 2010 |
|
RU2440313C1 |
HIGH-STRENGTH CONCRETE | 2015 |
|
RU2592322C1 |
METHOD FOR PREPARING CONCRETE MIX | 2022 |
|
RU2780905C1 |
METHOD FOR MODIFYING CONCRETE WITH COMPLEX ADDITIVE INCLUDING HYDROTHERMAL SIO2 NANOPARTICLES AND MULTILAYER CARBON NANOTUBES | 2020 |
|
RU2750497C1 |
Authors
Dates
2020-12-21—Published
2020-04-27—Filed