FIELD: construction.
SUBSTANCE: in the method to prepare a concrete mixture, consisting in mixing of cement, fillers, superplasticiser and mixing water, previously cement, fillers and a part of mixing water are mixed at the shop to produce a concrete mixture with slump of 2-4 cm, then the produced mixture is transported to a construction site, where a water solution of superplasticiser with remaining amount of mixing water is added in it not later than 2 hours from the moment of preparation, and the concrete mixture is finally mixed for at least 3 minutes.
EFFECT: improved convenience of laying, preservation of concrete mix mobility without reduction of concrete strength during all hardening times.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING CONCRETE MIXTURE | 2017 |
|
RU2656298C1 |
METHOD TO PREPARE CONCRETE MIX | 2014 |
|
RU2548263C1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2019 |
|
RU2730235C1 |
METHOD TO PREPARE CONCRETE MIX | 2014 |
|
RU2551546C1 |
METHOD OF PREPARING CONCRETE MIXTURE | 2019 |
|
RU2714895C1 |
COMPLEX ADDITIVE FOR CONCRETE MIXTURE | 2010 |
|
RU2457190C1 |
CONCRETE MIX MAKING METHOD | 2014 |
|
RU2559234C1 |
METHOD OF CONCRETE MIXTURE PREPARATION | 2014 |
|
RU2559235C1 |
COMPLEX ADDITIVE FOR CONCRETE MIXTURE | 2010 |
|
RU2432336C1 |
METHOD OF PREPARING CONCRETE MIXTURE FOR HIGH-STRENGTH CONCRETE | 2020 |
|
RU2739006C1 |
Authors
Dates
2012-02-27—Published
2010-12-02—Filed