FIELD: aviation and chemical industries. SUBSTANCE: aromatic polyamide fiber is treated preliminary by polar aprotic solvent (e.g. dimethylformamide or dimethylsulfoxide) or by mixture of polar aprotic and nonpolar solvent. Said treatment is carried out till shrinkage of the fiber is 0.5-5 of its origin length. Then solvent is removed of said fiber and fiber is impregnated by binder. The process is followed by molding with the help of common methods. Tear strength thus manufactured organoplasts is 960-2700 N/m. EFFECT: improves efficiency of the method. 3 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF POLYETHYLENE COATING | 1992 |
|
RU2005561C1 |
AMINO-DERIVATIVES OF C60-FULLERENE AND COMPOSITION MATERIAL COMPRISING INDICATED AMINO-DERIVATIVES | 2004 |
|
RU2254329C1 |
POLYMER BINDER, COMPOSITION MATERIAL BASED THEREON, AND A METHOD FOR PREPARATION THEREOF | 2001 |
|
RU2223988C2 |
COMPOSITION FOR PREPARING PREPREG | 1993 |
|
RU2105017C1 |
CHROMATOGRAPHIC POLYCAPILLARY COLUMN | 1999 |
|
RU2149397C1 |
PROCESS FOR PREPARING BIS-MALEIN IMIDEAMINE RESINS | 1991 |
|
RU2032696C1 |
MULTICHANNEL OPTICAL WAVEGUIDE (VERSIONS) | 2001 |
|
RU2200969C2 |
PREPREG | 2004 |
|
RU2264295C1 |
PREPREG AND ARTICLE MADE OF THE SAME | 2005 |
|
RU2278028C1 |
METHOD OF PLANT TREATMENT BY BIOLOGICALLY ACTIVE SUBSTANCE (VARIANTS) | 1994 |
|
RU2110917C1 |
Authors
Dates
1995-09-27—Published
1992-09-21—Filed