FIELD: artificial filaments. SUBSTANCE: method involves using isotactic polypropylene with average molecular weight 39500-59800 and mass-average molecular weight 273000-350000. Monofilament is drawn in two stages. Thermofixation of monofilament is performed by exposing it to live steam for 10-40 minutes at 110-140 C. EFFECT: improved biological compatibility. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR LAYER FABRICATION | 1992 |
|
RU2040649C1 |
TEXTILE FIBROUS BULKED CATALYST | 1997 |
|
RU2118908C1 |
METHOD OF PREPARING SUPERHIGH MOLECULAR POLYETHYLENE SOLUTION | 1997 |
|
RU2121483C1 |
METHOD OF PREPARING TEXTILE VOLUMINOUS FIBROUS CATALYST | 1998 |
|
RU2145653C1 |
FILTERING CLOTH FROM SYNTHETIC FIBERS | 1994 |
|
RU2106899C1 |
TECHNIQUE TO ANALYZE GEOMETRICAL STRUCTURAL PARAMETERS OF FABRIC | 2000 |
|
RU2164686C1 |
METHOD OF MANUFACTURING VISCOSE FIBERS | 1994 |
|
RU2096536C1 |
DIFFRACTIVE PROCEDURE DETERMINING NUMBER OF MAIN CHARACTERISTICS OF CLOTH AND CLOTH-LIKE MATERIALS | 2001 |
|
RU2199739C2 |
METHOD OF MANUFACTURING ION-EXCHANGE FIBER | 2000 |
|
RU2194809C2 |
METHOD OF PRODUCTION OF POLYCHROMATIC PATTERNS ON PRODUCT SURFACE | 1993 |
|
RU2045587C1 |
Authors
Dates
1995-11-10—Published
1993-07-27—Filed