FIELD: building materials production. SUBSTANCE: proposed binder contains (mass): cement 6.0-8.0, phosphogypsum being wastes of phosphorous fertilizer production 20.0-23.0, ash having specific surface 3500-4100 cm2/g 46.0-54.0, ground waste slate 20.0-23.0. Compressive strength thus prepared binder after hardening within 28 days is 11.0-11.91 MPa. EFFECT: improves quality of desired product. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDING COMPOSITION | 1991 |
|
RU2005697C1 |
MIXTURE OF MAKING LIGHT CONCRETE AND LIGHT CONCRETE | 2008 |
|
RU2399598C2 |
RAW MIXTURE FOR CELLULAR CONCRETE MAKING | 1999 |
|
RU2148050C1 |
METHOD OF OBTAINING UNBURNT MINERAL BINDING AGENT OF HYDRAULIC HARDENING | 2011 |
|
RU2476393C1 |
METHOD TO PREPARE ASH-CONCRETE MIX | 2013 |
|
RU2526072C1 |
ACTIVE MINERAL ADDITIVE FOR CEMENT AND METHOD FOR PREPARATION THEREOF | 2015 |
|
RU2581437C1 |
ASH-CEMENT BINDER (ZOLCIT) BASED ON ACID ASHES OF THERMAL POWER PLANTS | 2010 |
|
RU2452703C2 |
CRUDE MIXTURE FOR PRODUCING GYPSUM BINDER AND ARTICLES FROM SAID BINDER | 2009 |
|
RU2413688C2 |
METHOD FOR PREPARATION OF CONCRETE MIX | 2007 |
|
RU2351563C1 |
METHOD FOR PRODUCING BINDER FOR CONCRETE AND MORTAR MIXES | 2017 |
|
RU2664567C1 |
Authors
Dates
1995-12-10—Published
1992-02-11—Filed