FIELD: production of synthetic leather. SUBSTANCE: proposed composition contains (mass parts): polyvinyl chloride 100, polyester plasticizer 40-70, butadiene acrylonitrile rubber 10-30, mineral filler 0.3-16.0, metal-containing stabilizing agent 1-5, stearic acid 0.4-2.5, pigments 0.2-3.0, polyhexamethylene guanidine chloride 0.1-20.0. EFFECT: improves quality of desired product. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MULTILAYER MATERIAL | 2000 |
|
RU2171325C1 |
POLYMERIC COMPOSITION | 1991 |
|
RU2021308C1 |
MULTILAYER LEATHER | 1998 |
|
RU2147056C1 |
POLYVINYL CHLORIDE COMPOSITION FOR PRODUCING FILM MATERIALS | 2010 |
|
RU2429255C1 |
MULTILAYER MATERIAL | 2000 |
|
RU2169221C1 |
MULTILAYER MATERIAL | 2000 |
|
RU2169220C1 |
MULTILAYER MATERIAL | 2001 |
|
RU2194814C1 |
POLYMERIC COMPOSITION | 0 |
|
SU1553547A1 |
METHOD FOR MANUFACTURE OF FIRE-PROOF TWO-SIDED ANTISTATIC MATERIAL | 2000 |
|
RU2188760C2 |
COMPOSITION FOR THERMOHARDNESS ROLL MATERIAL EXTERNAL LAYERS | 1994 |
|
RU2098439C1 |
Authors
Dates
1995-12-20—Published
1990-10-12—Filed