FIELD: alloy production. SUBSTANCE: quartz sand is added to the aluminium melt in amount 20-25% calculated on the melt weight. The mixture obtained is treated at 800-850 C with products of the reaction of steam with a carbonaceous stuff for 15-20 min. After further 30-40 min the melt is poured out. The yield of silumine is 11-16% higher. EFFECT: increased silicium content. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING OF SLAGS OF SMELTING OF ALUMINIUM AND ITS ALLOYS | 1993 |
|
RU2061070C1 |
METHOD FOR PRODUCTION OF SILUMINES | 1996 |
|
RU2094515C1 |
METHOD FOR PRODUCING SILUMINS USING AMORPHOUS MICROSILICA | 2020 |
|
RU2754862C1 |
METHOD FOR PRODUCTION OF CAST ALUMINIUM-SILICON COMPOSITE ALLOY | 2014 |
|
RU2570142C1 |
METHOD OF SILUMINES PREPARATION | 0 |
|
SU1772198A1 |
METHOD OF OBTAINING SILUMIN | 2018 |
|
RU2683176C1 |
METHOD OF PREPARING BORON-CONTAINING HARDENER | 1993 |
|
RU2063459C1 |
METHOD OF PRODUCING SILUMINS IN ELECTROLYSIS CELL FOR PRODUCING ALUMINIUM | 2020 |
|
RU2736996C1 |
METHOD FOR MODIFICATION OF SILUMINS | 1993 |
|
RU2068016C1 |
METHOD OF PREPARING SILUMINS | 1993 |
|
RU2068015C1 |
Authors
Dates
1996-07-10—Published
1993-03-01—Filed