FIELD: electrometallurgy. SUBSTANCE: process of heat treatment of parts with electroplated nickel coating refers mainly to coatings made from dispersion-solidifying alloy. Process includes heating of parts up to specified temperature with rate not exceeding 200 C/h, first isothermic curing at temperature 150-200 C for the course of 60-90 min, subsequent heating, second isothermic curing at temperature of phase transformations in alloy at 810-875 C for the course of 60-90 min and cooling. EFFECT: enhanced efficiency of heat treatment. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF DEPOSITION OF PROTECTIVE COATS ON ARTICLES | 1994 |
|
RU2066715C1 |
TELESCOPIC STRUCTURE SOLDERING METHOD | 1998 |
|
RU2156182C2 |
METHOD OF HEAT TREATMENT OF STRUCTURES | 1997 |
|
RU2129166C1 |
METHOD OF SURFACING BUTT JOINED EDGES OF WORKPIECES | 1993 |
|
RU2063313C1 |
PART SOLDERING METHOD | 1993 |
|
RU2051013C1 |
PROCESS FOR MANUFACTURING CORRUGATED PIPES | 1993 |
|
RU2063284C1 |
METHOD OF MAKING SOLDERED TELESCOPIC STRUCTURES | 1996 |
|
RU2109606C1 |
POWDER CHARGE AND METHOD TO PRODUCE OUT OF IT PROTECTIVE METAL-CERAMIC COATING ON PIECES OF DISPERSION-HARDENING NICKLE ALLOYS | 1994 |
|
RU2078849C1 |
METHOD FOR SOLDERING REFRACTORY DISPERSION-HARDENED NICKEL-CHROME BASE ALLOYS | 1996 |
|
RU2129061C1 |
METHOD OF VACUUM ION-PLASMA COATING OF SUBSTRATE | 2000 |
|
RU2192501C2 |
Authors
Dates
1996-07-27—Published
1993-07-07—Filed